DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-06 | 7217304100 | WELDING WIRE FROM COPPER LOW ALLOY STEEL COATING CONTAINING LESS 0.25 MSS.% CARBON coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing | CHANGZHOU cHANGJIANG | CHINA | 52368 | 33599,76 | SHANGHAI | ***** | ***** |
2017-10-02 | 7217304100 | WELDING WIRE FROM COPPER LOW ALLOY STEEL COATING CONTAINING LESS 0.25 MSS.% CARBON coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing. APPLY FOR WELDING | CHANGZHOU cHANGJIANG | CHINA | 26106.4 | 16680,65 | SHANGHAI | ***** | ***** |
2017-10-04 | 7217304100 | Welding of low alloy steel with copper coating containing less than 0.25 wt.% Carbon, coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing, it is used for | DEKA | CHINA | 158102.72 | 133893,22 | QINGDAO | ***** | ***** |
2017-10-06 | 7217304100 | WELDING WIRE FROM COPPER LOW ALLOY STEEL COATING CONTAINING LESS 0.25 MSS.% CARBON coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing. APPLY FOR WELDING | CHANGZHOU cHANGJIANG | CHINA | 26318.4 | 16822,57 | SHANGHAI | ***** | ***** |
2017-10-08 | 7217304100 | Welding of low alloy steel with copper coating containing less than 0.25 wt.% Carbon, coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing, it is used for | DEKA | CHINA | 107960.32 | 98947,99 | TIANJIN | ***** | ***** |
2017-10-11 | 7217304100 | WIRE mild steel S235 STANDARDS SPEZI 20 / 90-6, OBMEDNENNAYA: diameter 4.5 mm, â„–054105, ART: M212472A1 - 10795 kg (11 coils). | WDI | GERMANY | 10795 | 9563,89 | Kaluga | ***** | ***** |
2017-10-12 | 7217304100 | MIG WELDING WIRE non-alloy steel with copper coating without a core, WITHOUT COVERING flux, the thickness of 1.2 mm in coils on the coil, CONTAINING CARBON 0.09% is used for semi-automatic welding in shielding gases | SUPERON | INDIA | 14010 | 15076,39 | GURGAON | ***** | ***** |
2017-10-13 | 7217304100 | Welding of low alloy steel with copper coating, containing less than 0.25 wt.% Carbon, coreless WITHOUT COATING fluxing. Is wound on a plastic coil-2674 PCS, made by a method of cold drawing, used for welding | ALFA MAG | CHINA | 44772 | 40577,86 | SHANGHAI | ***** | ***** |
2017-10-13 | 7217304100 | Welding of low alloy steel with copper coating, containing less than 0.25 wt.% Carbon, coreless WITHOUT COATING fluxing. Is wound on a plastic coil-12907 PCS, made by a method of cold drawing, used for welding | ALFA MAG | CHINA | 204632 | 197435,17 | SHANGHAI | ***** | ***** |
2017-10-16 | 7217304100 | WELDING WIRE FROM COPPER LOW ALLOY STEEL COATING CONTAINING LESS 0.25 MSS.% CARBON coreless WITHOUT COATING fluxing. Is wound on a plastic coil, made by a method of cold drawing. APPLY FOR WELDING | CHANGZHOU cHANGJIANG | CHINA | 26318.4 | 20036,73 | SHANGHAI | ***** | ***** |