2017-11-02 | 7601208009 | PRIMARY ALUMINUM ALLOY USED for further industrial processing, MARK A356.2 (SR) - 405000 kg in small pigs, tie plastic tape | RUSAL | USA | 2246000 | 5051371,61 | KRASNOYARSK | ***** | ***** |
2017-11-08 | 7601208009 | PRIMARY ALUMINUM ALLOY USED for further industrial processing, MARK A356.2 (SR) TECH. In SPETS.449-03-73 T / SHAPED chushka ENSHRINED WOODEN props | RUSAL | USA | 907000 | 1979147,88 | KRASNOYARSK | ***** | ***** |
2017-11-13 | 7601208009 | SAMPLES ALUMINUM ALLOY PRIMARY MARKS A356.2 (SR) for further analysis CONSUMER. SPECIFICATION TC 449-03-73 (23 samples). Tensile strength NOT reaches 240 MPa at 200 ° C or 415 MPa at 25 ° C. | *** | USA | 1.795 | 3,55 | KRASNOYARSK | ***** | ***** |
2017-11-13 | 7601208009 | PRIMARY ALUMINUM ALLOY USED for further industrial processing, MARK A356.2 (SR) The T / SHAPED chushka ENSHRINED WOODEN props TC 449-03-127 | RUSAL | USA | 63000 | 138621,89 | KRASNOYARSK | ***** | ***** |
2017-11-14 | 7601208009 | SAMPLES ALUMINUM ALLOY PRIMARY MARKS A356.2 (SR) DATA TS 449-03-73 (29 samples), TC 449-03-120 (80 samples), A356.2 BRAND CU 449-02-189 (55 SAMPLES) FOR FURTHER Consumer Analysis. Tensile strength FAILS | *** | USA | 17.835 | 35,39 | KRASNOYARSK | ***** | ***** |
2017-11-17 | 7601208009 | SAMPLES ALUMINUM ALLOY FOR PRIMARY MARKS A356.2 (SR) FURTHER ANALYSIS OF CONSUMER. SPECIFICATION TC 449-03-127 (27 samples). Tensile strength NOT reaches 240 MPa at 200 ° C or 415 MPa at 25 ° C. | *** | USA | 2.03 | 3,97 | KRASNOYARSK | ***** | ***** |
2017-11-22 | 7601208009 | PRIMARY ALUMINUM ALLOY USED for further industrial processing, MARK A356.2 (SR) TECH. SPECIALIST. 449-03-128 VT / SHAPED chushka ENSHRINED WOODEN props | RUSAL | USA | 147000 | 317663,39 | KRASNOYARSK | ***** | ***** |
2017-11-23 | 7601208009 | SAMPLES ALUMINUM ALLOY PRIMARY MARKS A356.2 (SR) for further analysis CONSUMER. SPECIFICATION TC 449-03-85 (48 samples). Tensile strength NOT reaches 240 MPa at 200 ° C or 415 MPa at 25 ° C. | *** | USA | 3.615 | 7,19 | KRASNOYARSK | ***** | ***** |
2017-11-23 | 7601208009 | SAMPLES aluminum alloy A356.2 GRADE PRIMARY for further analysis of the consumer. SPECIFICATION TC 449-03-107 (72 samples). Tensile strength NOT reaches 240 MPa at 200 ° C or 415 MPa at 25 ° C. | *** | USA | 5.395 | 10,74 | KRASNOYARSK | ***** | ***** |
2017-11-24 | 7601208009 | SAMPLES ALUMINUM ALLOY PRIMARY MARKS A356.2 (SR) DATA TS 449-02-181 (105 SAMPLES) TC 449-03-120 (75 samples), A356.2 BRAND CU 449-02-189 (55 SAMPLES) FOR FURTHER Consumer Analysis. Tensile strength not | *** | USA | 23.025 | 46,24 | KRASNOYARSK | ***** | ***** |