DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-11-02 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM LESS THAN 0.85% C tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 27002KG (3185 pigs) | ABSENT | JAPAN | 27002 | 47928,55 | Novorossiysk | ***** | ***** |
2017-11-08 | 7601208002 | SECONDARY ALUMINUM ALLOYS, RAW, bullion TYPE AK5 M2 - 1776SHT, CONTAINING MAC 4.004-5.210% SI, 0.922-1.397 MSS% CU, 0.362-0.498 MSS% MG, 0.511-0.990 MSS% ZN, 0.191-0.277 MSS% MN , MAC 0.839-0.991% FE, 0.049-0.122 MAC% NI, 0. | ABSENT | JAPAN | 26979 | 48157,52 | Novorossiysk | ***** | ***** |
2017-11-10 | 7601208002 | SECONDARY ALUMINUM ALLOYS, RAW, bullion TYPE AK5 M2 - 1809SHT, CONTAINING MAC 3.867-5.981% SI, 0.979-1.378 MSS% CU, 0.401-0.498 MSS% MG, 0.711-0.990 MSS% ZN, 0.192-0.277 MSS% MN , MAC 0.875-0.992% FE, 0.049-0.136 MAC% NI, 0. | ABSENT | JAPAN | 26986 | 48170,01 | Novorossiysk | ***** | ***** |
2017-11-17 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM less than 0.5% C, the tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 54090KG (6288 pigs) | ABSENT | JAPAN | 54090 | 96550,65 | Novorossiysk | ***** | ***** |
2017-11-20 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM less than 0.5% C, the tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 54002KG (6233 pigs) | ABSENT | JAPAN | 54002 | 97203,6 | Novorossiysk | ***** | ***** |
2017-11-20 | 7601208002 | SECONDARY ALUMINUM ALLOYS, RAW, bullion TYPE AK5 M2 - 1793SHT, CONTAINING MAC 3.022-5.553% SI, 0.885-1.328 MSS% CU, 0.326-0.499 MSS% MG, 0.635-0.998 MSS% ZN, 0.173-0.304 MSS% MN , MAC 0.781-0.955% FE, 0.061-0.136 MAC% NI, 0. | ABSENT | JAPAN | 26984 | 48301,36 | Novorossiysk | ***** | ***** |
2017-11-22 | 7601208002 | SECONDARY ALUMINUM ALLOYS, RAW, bullion TYPE AK5 M2 - 1751SHT, CONTAINING MAC 3.014-5.311% SI, 0.937-1.234 MSS% CU, 0.352-0.497 MSS% MG, 0.805-0.994 MSS% ZN, 0.208-0.335 MSS% MN , MAC 0.889-0.988% FE, 0.075-0.188 MAC% NI, 0. | ABSENT | JAPAN | 26990 | 48312,1 | Novorossiysk | ***** | ***** |
2017-11-24 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM less than 0.5% C, the tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 108012KG (12624 pigs) | ABSENT | JAPAN | 108012 | 194421,6 | Novorossiysk | ***** | ***** |
2017-11-27 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM less than 0.5% C, the tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 54001KG (6166 pigs) | ABSENT | JAPAN | 54001 | 98011,82 | Novorossiysk | ***** | ***** |
2017-11-30 | 7601208009 | ALUMINUM ALLOYS, SECONDARY, RAW, foundry ingots GRADE TYPE AK5M2 SOD.TSINKA C less than 1.0% SOD. MAGNESIUM less than 0.5% C, the tensile strength LESS 170MPA (IF TEMPER.25 degrees C) GOST1583-93- 54026KG (6096 pigs) | ABSENT | JAPAN | 54026 | 97246,8 | Novorossiysk | ***** | ***** |