DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-04 | 7325910000 | CYLINDER CHUGUNNYE grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and the HLR. MATERIALS 35x35 C 3,17%; SI 1,90%; S 0,075%; Hardness HRC 47.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10552,99 | PPASHIYA | ***** | ***** |
2017-10-04 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,81%; S 0,144%; Hardness HRC 47.5 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10445,59 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,81%; S 0,144%; Hardness HRC 47.5 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10467,35 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,10%; SI 1,97%; S 0,126%; Hardness HRC 46.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10467,35 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,96%; S 0,139%; Hardness HRC 48.7 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10141,27 | PPASHIYA | ***** | ***** |
2017-10-09 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,10%; SI 1,97%; S 0,126%; Hardness HRC 46.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10095,94 | PPASHIYA | ***** | ***** |
2017-10-10 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,04%; SI 1,64%; S 0,112%; Hardness HRC 47.6 CM. ATTACHMENT OBTAINED PROTSESSOM CASTING is not no OECs | ABSENT | POLAND | 21000 | 10103,45 | PPASHIYA | ***** | ***** |
2017-10-10 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,05%; SI 1,68%; S 0,123%; Hardness HRC 47.9 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10103,45 | PPASHIYA | ***** | ***** |
2017-10-13 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,48%; SI 1,70%; S 0,145%; Hardness HRC 47.9 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10220,77 | PPASHIYA | ***** | ***** |
2017-10-23 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,00%; SI 1,85%; S 0,149%; Hardness HRC 47.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10183,83 | PPASHIYA | ***** | ***** |