DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-04 | 7325910000 | CYLINDER CHUGUNNYE grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and the HLR. MATERIALS 35x35 C 3,17%; SI 1,90%; S 0,075%; Hardness HRC 47.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10552,99 | PPASHIYA | ***** | ***** |
2017-09-06 | 7326909807 | TUBA INPUT 89550684-1SHT, steel structural elements of complex geometric shapes in the form of a cylinder is mounted on the cigarette LINE "FOCKE" and are intended for guiding the cigarette rod, VNESH.DIAMETR 17mm, height 16mm, METHOD | ABSENT | POLAND | 0.018 | 900,45 | August | ***** | ***** |
2017-09-06 | 7326909807 | TUBA OUTPUT 89550685-1SHT, steel structural elements of complex geometric shapes in the form of a cylinder is mounted on the cigarette LINE "FOCKE", designed to direct MOTION cigarette rod, VNESH.DIAMETR 17mm, height 16mm, METHOD | ABSENT | POLAND | 0.02 | 1012,97 | August | ***** | ***** |
2017-10-04 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,81%; S 0,144%; Hardness HRC 47.5 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10445,59 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,81%; S 0,144%; Hardness HRC 47.5 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10467,35 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,10%; SI 1,97%; S 0,126%; Hardness HRC 46.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 22500 | 10467,35 | PPASHIYA | ***** | ***** |
2017-10-05 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,03%; SI 1,96%; S 0,139%; Hardness HRC 48.7 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10141,27 | PPASHIYA | ***** | ***** |
2017-10-05 | 7306301100 | Welded, COLD PRECISION for hydraulic cylinders, without thread; UGLEROD.STAL E235; STANDARD EN10305; SIZE 18.5 * 1.25MM.TRUBY not double multiwall NOT, NOT FOR NUCLEAR REACTORS | ABSENT | POLAND | 7195 | 8247,69 | Pervouralsk | ***** | ***** |
2017-10-09 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,10%; SI 1,97%; S 0,126%; Hardness HRC 46.6 CM. ATTACHMENT OBTAINED casting process is not no OECs | ABSENT | POLAND | 21000 | 10095,94 | PPASHIYA | ***** | ***** |
2017-10-10 | 7325910000 | CAST IRON CYLINDER grinding for ball mills (cylpebs) HELD FOR ball milling coal clinker and DR. MATERIALS 35x35 C 3,04%; SI 1,64%; S 0,112%; Hardness HRC 47.6 CM. ATTACHMENT OBTAINED PROTSESSOM CASTING is not no OECs | ABSENT | POLAND | 21000 | 10103,45 | PPASHIYA | ***** | ***** |