DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-01 | 2506100000 | Quartz concentrate a quartz grits (fraction less than 25 um, 25-100MKM more 100um) obtained by crushing and manual sorting laundered vein quartz, after magnetic concentration, flotation, washing, drying and packaging. AVAILABLE free of charge | ABSENT | KINGDOM OF THE NETHERLANDS | 500 | 617,27 | Winschoten | ***** | ***** |
2017-09-08 | 2506100000 | Quartz concentrate a quartz grits (fraction less than 100um, 100-300MKM more 300MKM) obtained by crushing and manual sorting laundered vein quartz, after magnetic concentration, flotation, washing, drying and packaging. | ABSENT | KINGDOM OF THE NETHERLANDS | 20000 | 26319,39 | Winschoten | ***** | ***** |
2017-09-15 | 2506100000 | Quartz concentrate a quartz grits (fraction less than 100um, 100-300MKM more 300MKM) obtained by crushing and manual sorting laundered vein quartz, after magnetic concentration, flotation, washing, drying and packaging. | ABSENT | KINGDOM OF THE NETHERLANDS | 20000 | 26731,57 | Winschoten | ***** | ***** |
2017-09-22 | 2506100000 | QUARTZ concentrate obtained SORT laundered vein quartz and remote MINERALOGICAL impurities and produce a working FRACTION 100-300 MCM by crushing, screening and dry magnetic separation, flotation - 20000 kg. | UNKNOWN | KINGDOM OF THE NETHERLANDS | 20000 | 26614,5 | WINSCHOTEN | ***** | ***** |
2017-09-27 | 2506100000 | QUARTZ concentrate obtained SORT laundered vein quartz and remote MINERALOGICAL impurities and produce a working FRACTION 0.1-0.3 MM. By crushing, screening and dry magnetic separation, flotation - 20000 kg. | UNKNOWN | CHINA | 20000 | 59040 | SHANGHAI | ***** | ***** |
2017-09-27 | 2506100000 | QUARTZ concentrate obtained SORT laundered vein quartz and remote MINERALOGICAL impurities and produce a working FRACTION 0.1-0.3 MM. By crushing, screening and dry magnetic separation, flotation - 40000 kg. | UNKNOWN | CHINA | 40000 | 72200 | SHANGHAI | ***** | ***** |
2017-09-29 | 2506100000 | QUARTZ concentrate obtained SORT laundered vein quartz and remote MINERALOGICAL impurities and produce a working FRACTION 100-300 MCM by crushing, screening and dry magnetic separation, flotation - 20000 kg. | UNKNOWN | KINGDOM OF THE NETHERLANDS | 20000 | 26614,5 | WINSCHOTEN | ***** | ***** |