2017-11-02 | 7225199000 | Cold-rolled steel ELECTRIC siliceous alloyed rolls, 2 rolls, SI-1.41%, AL-0.34%, C-0.007%, tensile strength 420 MPA | "Severstal" | EGYPT | 16860 | 5359,29 | ST PETERSBURG | ***** | ***** |
2017-11-02 | 7225309000 | The hot-rolled steel ROLLS doped ROLLS 7, TI-0.062%, CR-0.66%, MO-0.12, 0.122%, SI-1.36%, tensile strength 377-570 MPa | "Severstal" | EGYPT | 185820 | 59066,6 | ST PETERSBURG | ***** | ***** |
2017-11-02 | 7225990000 | Hot-rolled steel pickling / alloyed corrugated rolls, 2 rolls, SI-0.65%, NB-0.061%, a tensile strength of 500 558 MPa | Severstal | EGYPT | 41650 | 16198,48 | ST PETERSBURG | ***** | ***** |
2017-11-13 | 7225920000 | GALVANIZED STEEL IN ROLLS doped with C = 0.004%, TI = 0.07%, NI = 0.001%, tensile strength 362 N / MM2 1 ROLL | "Severstal" | EGYPT | 2930 | 930,25 | ST PETERSBURG | ***** | ***** |
2017-11-13 | 7225920000 | GALVANIZED STEEL IN ROLLS doped ROLL 2, TI-0.069, 0.073%, tensile strength 307 MPA 309 | "Severstal" | EGYPT | 16470 | 5229,06 | ST PETERSBURG | ***** | ***** |
2017-11-13 | 7225404000 | The alloyed hot-rolled steel sheet with = 0.058-0.065%, NI = 0.37-0.4%, MO = 0.15-0.177% Tensile strength 570-605 MPa 20 SHEETS | "Severstal" | EGYPT | 186931 | 68803,69 | ST PETERSBURG | ***** | ***** |
2017-11-14 | 7225404000 | The alloyed hot-rolled steel sheet with = 0.049-0.067%, NI = 0.21-0.29%, MO = 0.155-0.25%, MN = 1.73-1.88%, NB = 0.066% Tensile strength 600-720 MPa 114 SHEETS | "Severstal" | EGYPT | 608179 | 223730,81 | ST PETERSBURG | ***** | ***** |