DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-11-11 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938): from 60.6 to 62.4 degrees C; Density at 70 degrees C (Method ASTM D 1298): from 0.8133 to 0.8147 g / cm3; Penetration index (method ASTM D 217) at 25 | "LUKOIL" | LITHUANIA | 196714 | 108453,45 | STGUDOGAY | ***** | ***** |
2017-11-11 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938): from 60.6 to 62.2 degrees C; Density at 70 degrees C (Method ASTM D 1298): 0.8147 g / cm3; Penetration index (method ASTM D 217) at 25 degrees C: 44 and | "LUKOIL" | LITHUANIA | 193919 | 106912,5 | STGUDOGAY | ***** | ***** |
2017-11-13 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938): 62.0 degrees C, density at 70 degrees C (Method ASTM D 1298): 0.8142 g / cm3, a penetration index (method ASTM D 217) at 25 degrees C: 46. | "LUKOIL" | LITHUANIA | 49713 | 26814,5 | STGUDOGAY | ***** | ***** |
2017-11-13 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938): 62.4 degrees C, density at 70 degrees C (Method ASTM D 1298): 0.8133 g / cm3, a penetration index (method ASTM D 217) at 25 degrees C: 46. | "LUKOIL" | LITHUANIA | 49396 | 26643,51 | STGUDOGAY | ***** | ***** |
2017-11-13 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938): 62.4 degrees C, density at 70 degrees C (Method ASTM D 1298): 0.8133 g / cm3, a penetration index (method ASTM D 217) at 25 degrees C: 46. | "LUKOIL" | LITHUANIA | 48738 | 26288,59 | STGUDOGAY | ***** | ***** |
2017-11-14 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938) not lower than 30 degrees C, | "LUKOIL" | LITHUANIA | 100000 | 57060,51 | STGUDOGAY | ***** | ***** |
2017-11-29 | 2712903900 | Slack resulting from dewaxing of lubricating oils. CRYSTALLIZATION TEMPERATURE (METHOD ASTM D 938) not lower than 30 degrees C, density at 70 degrees C (Method ASTM D 1298): less than 0.942 g / cm3, a penetration index (method ASTM D 217) at 25 degrees C: | "LUKOIL" | LITHUANIA | 100000 | 59485,04 | STGUDOGAY | ***** | ***** |
2017-11-30 | 2712903900 | TSEREZIN.MARKA 75. RAW. INTENDED FOR greases, wax alloys, insulation materials and other purposes. BULK. | ABSENT | LITHUANIA | 52300 | 57705,3 | ST RED | ***** | ***** |